Speaker pursuit road > woodwork painting technology the chapter top >
Basic program of works of varnish painting
No. | Process | Employed material | Processing method | Leaving time |
1 | Foundation adjustment | The 240th grinding | Exterminating and foundation grinding of defect | - |
2 | Coloring | Kibe colorant | It smears on wood and it wipes off though it is Wess and the imprinting at once. | One hour or more |
3 | Undercoat | Varnish | Brush paint that dilutes and calms down | One hour or more |
4 | Grinding | Grinding | The supplementation with the following page is seen. | - |
5 | Final coating | Varnish | It becomes finished that you may thin by the reducer a little. |
It is a basic program of works. Please omit "Color" of No2 when finishing it up by a clear color. It becomes more beautiful more finished by repeating the process of 3 and 4 2 and three times. You may thin the density of the varnish a little by the final finish (The amount in which the reducer is mixed is increased).
When the woodwork painting is examined on the net, it is understood that there is considerably misunderstand big being done. The barrel one is the one "The woodwork painting goes well when paints are thinned as much as possible and the piling paint is done a lot". This is a complete mistake. Do not dilute it because it does to make it to thickness at the undercoat of being in the process below (It undertakes the undercoat and intermediate coat when it goes from the original woodwork painting process). With this, the paint film doesn't attach. Only when the last final coating (finish paint) is done, diluting it is good.